Platinum • Transition Metal

Primary XPS region: Pt4f
Overlapping regions: Al2p
Binding energies of common chemical states:

Chemical stateBinding energy Pt4f7/2
Pt metal71.0 eV
PtO72.4 eV
PtO274.9 eV

 

Interpretation of XPS spectra
  • Pt4f region has well separated spin-orbit components (Δmetal=3.35eV).
    • Peaks in the Pt4f region have an asymmetric peak shape for platinum metal.
    • Platinum compounds, such as the oxide, have symmetric Pt4f peaks.

 

About this element
Element Crystal cub

Symbol: Pt
Date of discovery: 1735
Name origin: Spanish platina
Appearance: silver
Discoverer: Julius Scaliger
Obtained from: platinum ores

Melting point: 2041 K
Boiling point: 4098 K
Density[kg/m3]: 21090
Molar volume: 9.09 × 10-6 m3/mol
Protons/Electrons: 78
Neutrons: 117
Shell structure: 2,8,18,32,17,1
Electron configuration: [Xe]4f145d96s1
Oxidation state:  2,4
Crystal structure: cubic

Discovered by J. Scaliger in 1735, platinum is a beautiful, gray-white metal that is malleable in its pure form. It is extremely resistant to corrosion and tarnishing, and will not oxidize in air, even at high temperatures. Platinum is very rare, and is naturally found as the uncombined metal. Because of its extreme durability and resistance to tarnishing, platinum is widely used to make jewelry. It is also used to make surgical tools, liquid crystal displays, and electrical resistance wires. Platinum is named for the Spanish word “platina,” meaning “little silver.”

element_platinum

Products

Nexsa G2 XPS

  • Micro-focus X-ray sources
  • Unique multi-technique options
  • Dual-mode ion source for monoatomic & cluster ion depth profiling
Style Sheet for Instrument Cards Original

K-Alpha XPS

  • High resolution XPS
  • Fast, efficient, automated workflow
  • Ion source for depth profiling

ESCALAB QXi XPS

  • High spectral resolution
  • Multi-technique surface analysis
  • Extensive sample preparation and expansion options

Contact us

Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
Style Sheet for Products Table Specifications
Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
Style Sheet for Products Table Specifications
Fix for left nav
Style Sheet for Support and Service footer
Style Sheet for Fonts
Style Sheet for Cards

Electron microscopy services for
the materials science

To ensure optimal system performance, we provide you access to a world-class network of field service experts, technical support, and certified spare parts.